At Klandee R&E, we deliver Metallurgical Coal of various specifications and sizes, customized to meet the requirements of the clients with whom we maintain long term relationships. With the economy looking very buoyant the demand outlook for superior quality Metallurgical Coal is positive and the company strives to bridge the demand supply gap by adding fresh capacity and manufacture high quality Metallurgical Coal.
Specification – (Klandee – SSCC-AUS) |
Typical Quality (%) |
---|---|
Coking Properties | |
Crucible Swelling Number (CSN) | 5.5 |
Proximate Analysis | |
Volatile Matter (VM) | 34 (air dried) |
Ash | 9.25 (air dried) |
Phosphorous (P) | 0.025 (air dried) |
Sulfur (S) | 0.58 (air dried) |
Fixed Carbon | 53 |
Total Moisture (TM) | 9.5 (as received) |
Specification – (Klandee – PCI-A12-AUS) |
Typical Quality (%) |
---|---|
Proximate Analysis | |
Volatile Matter (VM) | 15 (air dried) |
Ash | 12 (air dried) |
HGI | 78 |
Sulfur (S) | 0.55 (air dried) |
Total Carbon | 90.5 dry, ash free |

Specification – (Klandee – HCC 64 Mid Vol) |
Typical Quality (%) |
---|---|
Coking Properties | |
Coke Strength after Reaction (CSR) | 64 |
Maximum Fluidity | 1700ddpm |
Proximate Analysis | |
Volatile Matter (VM) | 25.5 (air dried) |
Ash | 9 (air dried) |
Phosphorous (P) | 0.05 (air dried) |
Chemical Analysis | |
Sulfur (S) | 0.6 (air dried) |
Moisture | |
Total Moisture (TM) | 9.5 (as received) |
Specification – (Klandee – Premium Low Vol) |
Typical Quality (%) |
---|---|
Coking Properties | |
Coke Strength after Reaction (CSR) | 71 |
Maximum Fluidity | 500ddpm |
Proximate Analysis | |
Volatile Matter (VM) | 21.5 (air dried) |
Ash | 9.3 (air dried) |
Phosphorous (P) | 0.0045 (air dried) |
Chemical Analysis | |
Sulfur (S) | 0.5 (air dried) |
Moisture | |
Total Moisture (TM) | 9.7 (as received) |
Specification – (Klandee – PDR) |
Typical Quality (%) |
---|---|
Coking Properties | |
Coke Strength after Reaction (CSR) | 74 |
Maximum Fluidity | 400ddpm |
Crucible Swell Number (CSN) | 8.5 |
Proximate Analysis | |
Volatile Matter (VM) | 20.7 (air dried) |
Ash | 10.5 (air dried) |
Phosphorous (P) | 0.030(air dried) |
Chemical Analysis | |
Sulfur (S) | 0.6 (air dried) |
Moisture | |
Total Moisture (TM) | 9.5 (as received) |
Maceral Analysis | |
Vitrinite | 68 |
Rank: Mean Max Reflectance | Ro Max 1.42 |